Spot welding of two steel sheets each 2 mm thick carried out successfully by passing 4 kA of current for 0.2 seconds through the electrodes. The resulting weld nugget formed between the sheets is 5 mm in diameter. Assuming cylindrical shape for the nugget, the thickness of the nugget is ______mm.
Latent heat of fusion for steel
|
1400 kJ/kg
|
Effective resistance of the weld joint
|
200 W
|
Density of steel
|
8000 kg/m3
|